Call 01493 277103

Lead roofing

Why Does Lead Flashing Crack?

Lead does not rust, so a cracked flashing has been stressed beyond what the sheet could take. Movement, size and fixing are the causes to look at, and each is explained here with what a repair involves.

Get a written quote

Call 01493 277103WhatsApp us

Lead-lined roof valley between two clay-tiled slopes, a few leaves caught in it

The short answer

Lead flashing cracks when it is stretched and squeezed by the weather more than the sheet can take. Pieces cut too long, fixings that grip too tightly, a code too thin for the detail and repeated bending all lead to splits. Cracked lead is mended or replaced, and the cause is dealt with too.

Lead moves with the weather

Lead is a soft metal, and like every metal it expands as it warms and shrinks as it cools. On a roof that happens every day and every season. A flashing is meant to slide a little along its fixings, and to flex at its folds, so that this movement is absorbed rather than resisted.

When the lead cannot move freely, the stress has to go somewhere. It collects at the folds, at the corners and at the points where the lead is fixed, and eventually the metal splits there. The fault is one of fatigue: each cycle of heat and cold bends the sheet a little, and a crack appears at the place where the bending has been repeated. A split along a fold is the clearest picture of this.

Lead is graded by code, and the specification sets the code for each detail, which is the starting point for avoiding cracks. A thin code over a long run invites splits, because the longer the piece, the further it travels with each change of temperature and the harder the stress hits its ends and folds.

The causes of cracks

Cracks trace back to a short list of faults, and several of them lie in how the lead was cut and fixed, not in the metal itself.

  • Pieces cut too long. A long length of lead moves further than a short one, and the stress at each end grows with it.
  • Fixings that hold too tightly, so the sheet cannot slide and splits where it is pinned.
  • Sheet too thin for the job, as when light lead covers a large exposed area.
  • Folds bent sharply, or bent back and forth, which fatigues the metal along the line of the fold.
  • Laps cut too short, so each piece ends up carrying strain that should have been shared.
  • Damage from being walked on, or from a tile that has dropped onto the lead.

Old age plays a part in some cracks, but age alone is not the explanation. MyJobQuote says correctly installed lead flashing can last for over 80 years, so a crack in a young flashing is worth checking against how it was cut and fixed.

How a crack is dealt with

What is done about a crack depends on how far it goes. A single short split in otherwise sound lead can take a patch, and our answer on patching lead on a roof compares a fused lead patch with tape and sealant. A crack that runs along a fold, or several cracks on one flashing, suggest the sheet has been over-stressed and may need replacing. Where the crack sits at a corner or an edge, the shape of the piece needs looking at as well as the sheet.

Replacing means more than swapping the metal. If the new piece is cut to the same long length and fixed the same tight way, it will crack in the same place. The cause has to change as well: shorter pieces, fixings that let the lead slide, clips at the lower edge and, where the detail calls for it, a heavier code.

Sealant is no answer to a crack, because it is bonded to a sheet that keeps moving, and mastic on lead flashing is covered by our separate page. The decision between mending and renewing is set out under repair or replace lead flashing.

Spotting a crack before it leaks

A crack does not always show as a leak straight away. A hairline split can let a little water through in driving rain and nothing in a light shower, which makes the stain indoors come and go and the cause hard to pin down. It is worth looking at the lead when a stain appears and disappears on a pattern of heavy rain. Looking at the lead on a dry day also shows hairlines more clearly than in rain.

Do not go onto the roof to look for one. Photograph the stain indoors, study the flashing through binoculars from the ground, and send a picture to our WhatsApp number or ask for a survey. The lead, the wall and the covering around it are examined together, and you hear about anything else seen.

You then receive one written price for the work. If you want the wider picture on lead work, the lead roofing and leadwork hub lists each guide, and the page on the signs your lead flashing has failed lists what to look for.

Questions and answers

Why has new lead flashing cracked already?

A crack in new lead points to the fitting: a piece cut too long, fixings that hold it too tightly, a code too thin for the detail or a sharp fold. The metal has not aged, so the stress came from how it was installed, and the same fault will recur if only the lead is swapped.

Can a cracked flashing be welded?

A short split can be mended with a fused lead patch, which is a form of lead welding. It only holds if the cause is dealt with too, because a sheet that keeps moving will crack again beside the repair. Our page on lead welding covers the technique and the flame safety involved.

Does a hairline crack matter if there is no leak?

It is a fault in the waterproofing, and a hairline can widen with each cycle of heat and cold. Whether it is mended now or watched is a decision for the survey, which looks at how long the split is, where it sits and what the lead around it is like.

Get a written quote

Tell us about your roof

Hand dressing a lead ridge roll with a wooden bossing stick

10-year workmanship guarantee, in writing

Call WhatsApp Written quote