The short answer
Only as a stopgap. A bead of mastic can close a small gap for a time, yet it does not repair split lead, a lifted edge or crumbled pointing, and it cannot follow the lead as the temperature moves it. A flashing that needs mastic to stay dry has a fault that wants a proper repair.
What mastic does on a flashing
Mastic is a soft, rubbery sealant, sold in cartridges, that fills a gap and skins over. On a lead flashing it gets run along the upper edge against the wall, or smeared over a split or a lifted corner. For a few weeks or months it can keep rain out of the gap it covers.
That is all it does. It sits on the surface of the problem. It does not make split lead whole, it does not hold a lifted edge down against the wind, and it does not put back the mortar that has crumbled round the head of the flashing.
A sealant bead on lead has no set life in years. Treat any claim of a set number of years with caution, since the answer turns on the product, the sun and how much the joint moves.
The sound approach is to treat sealant as a cosmetic layer at most, never as the thing that keeps the junction watertight.
Why mastic fails on lead
Lead moves. Sheet exposed to sun and cold expands and contracts, and a flashing is meant to slide a small distance along its fixings as it does. A bead of sealant bonded to both the lead and the brickwork has to stretch each time, and as it ages it hardens, lets go of one side and opens a hairline gap.
- The bond lets go of the lead, because rolled lead has a smooth, slightly oxidised skin.
- The sealant hardens and cracks in sunlight, along the very line where the lead moves.
- Water gets behind the bead and is held there, so the gap leaks and stays damp.
- The wall behind may be damp or crumbling, so the sealant has no sound face to stick to.
A second problem is that mastic hides the fault. A flashing wearing a layer of sealant is harder to inspect, and the next person to look at it has to scrape the bead away to see whether the lead beneath has split. Sealant also gives a false sense that the job is done, because the stain indoors may stop for a few dry weeks and return with the next heavy rain.
What a proper junction looks like
A lead flashing at a chimney or wall is held in two ways. Its upper edge is tucked into a joint raked out of the brickwork, wedged with small lead wedges and pointed up with mortar so the wall grips it. Its lower edge lies over the covering, with clips holding it down against the wind while leaving it free to move.
Our guide to types of lead flashing shows each piece. Pointing, wedges and clips are the working parts, and when one fails the repair is to that part: re-point the joint, re-dress and clip the edge, or patch or replace split lead.
Sealant is sometimes a sensible extra on top of that work, filling a hairline at an awkward corner. Used alone, in place of the joint, it is a cosmetic layer. If a chimney's flashing has been sealed more than once, that history suggests it has been failing for some time. Where a gap has opened because the lead has slid or split, no amount of sealant restores it.
If your flashing already has mastic on it
Mastic on a flashing says something useful: someone found a gap and tried to close it. Photograph the junction from the ground, note any stain indoors, and ask for a survey to find out what the bead is covering up. Do not scrape it off from a ladder, because that is how both the lead and the person get damaged.
At a survey, the sealant is cleared from the part being looked at so the lead, the joint and the wall can be seen. You get a straight answer on whether it is a re-point, a patch or new lead. The page on repair or replace lead flashing explains how that call is made, and the lead patch repair page covers small splits.
Our written quotes come as one total price. If scaffolding is needed for the work, we arrange the licence with our scaffolder where it stands on the highway. For the wider set of lead jobs, start at the lead roofing and leadwork hub, which links the guides on codes, flat roofs and valleys.