What Is Cut-Edge Corrosion?

Rust along the cut edge of a profiled steel sheet is a coating problem that has reached the metal. This page covers how to recognise it, what slows it down and when treatment stops being enough.

Get a written quote

Call 01493 277103WhatsApp us

Roofers fitting profiled metal sheets on a low-pitched roof

The short answer

Cut-edge corrosion is rust that begins at the raw steel edge of a coated roof sheet, where cutting removed the protective layers. It shows as orange staining and lifting paint along edges and laps, and it can be treated while the steel is sound. Past that point the sheet is replaced.

Where the rust starts and why

A profiled steel roof sheet leaves the factory with a zinc coating and a paint finish over the steel. Every cut through that sheet exposes a thin strip of bare steel, and the coating no longer seals it. Moisture sits against that strip, the steel rusts, and the rust pushes under the paint beside it.

Cuts happen in more places than the sheet ends. A sheet is trimmed where it meets a rooflight, around a flue or a vent pipe, at a hip or a valley, and at the eaves where it overhangs the gutter. Fixing holes are cut edges too, in miniature. Each is a place where the factory coating stops short of the metal.

The rust also needs somewhere to hold water. Overlaps between sheets, the underside of an eaves edge and the line where a sheet sits in a gutter all keep a film of damp against the metal for longer than an open, sloping face does. That is why an edge in a lap can be badly corroded while the flat of the sheet beside it still looks sound.

What shows from the ground and from the access hatch

  • Orange or brown streaks running down the profile from an edge.
  • Paint that has lifted or blistered in a narrow band along a cut.
  • Rust staining on the gutter below an overhanging edge.
  • Rust rings round fixings, flue collars and rooflight surrounds.
  • Flakes of coating lying in the gutter after rain.

These marks are the visible end of damage that began under the paint. A surface that looks only stained can already have lost thickness at the edge, which is why a survey checks the metal as well as the colour, tapping and probing the edge rather than judging it from a distance.

If the sheets run through to the inside, a lining or ceiling below may show brown water marks near the same edges. That points to rust that has gone through the sheet, not only along its edge, and it moves the job from coating repair towards replacing sheets.

Rooflights deserve a look as well. Where a plastic rooflight panel sits in a steel sheet, the cut in the steel around it is a long edge with fixings along it, and rust there can undermine the seal as well as the sheet.

Treatment, and the point where replacement takes over

Where the steel is still sound, the repair is a sequence on each affected edge. Loose rust and flaking coating are cleaned back to a firm surface, a rust treatment goes onto the exposed steel, and a protective coating is applied over the edge and a short strip of sheet either side. The aim is to seal the cut again so moisture cannot sit against raw metal.

That repair holds only while there is enough steel left to carry it. If an edge has rusted through, if holes have opened along a lap, or if the sheet flexes where it should be stiff, coating over it does nothing structural. The options then are a new sheet in the damaged bay or a new covering over the old. Our page on industrial roof cladding explains how sheets, liners and fixings go together.

Which route suits a roof is a finding from the survey, taken sheet by sheet and edge by edge rather than assumed for the whole building. A roof can need a coating repair on its south slope and new sheets over a loading bay, and the two are priced together as one job.

Keeping watch, and how we approach it

Because cut-edge corrosion starts small, it suits a routine look. Edges at the eaves and around rooflights can be reached from a safe position, and a check of those spots shows whether the coating is holding. Our page on commercial roof maintenance sets out what a maintenance visit covers.

Before we quote, we go over the whole roof, so the rusted edge you rang about is seen alongside the laps, fixings, rooflights and gutters around it. Anything else we spot is named in plain words. One written price then covers the work, and the building's wider roofing needs are listed under commercial roofing.

Access matters on a steel roof. A sheet weakened by rust can fail under a person's weight, so the survey and any repair plan start from how the roof can be reached and worked on safely, before anyone judges the rust itself. Fragile roof safety, a subject of its own, is covered in our fragile roof safety page.

Questions and answers

Is cut-edge corrosion fixed by painting over the rust?

Paint applied over loose rust and flaking coating does not stop the rusting underneath, because moisture is still sealed against bad metal. The edge needs cleaning back to a firm surface and a rust treatment before any protective coating goes on. If the steel has already lost thickness, no coating restores it.

Can I send a photo of rusty roof edges first?

Yes. A photo on WhatsApp shows the pattern of staining and where the sheet edges sit, which helps us plan the survey. It cannot show how much steel is left under the paint or whether the rust has reached a lap, so any number from us waits for the survey, and arrives as one price in writing.

What does treating cut-edge corrosion cost?

The cost turns on the number of edges affected, how far the rust has gone, whether sheets need replacing and how the roof is reached. Edges differ too much for a rate per edge to be fair, and a short run of light rust costs far less than a long lap rusted through, so the survey comes first and the price in writing covers whatever work it finds necessary.

Get a written quote

Tell us about your roof

Hand dressing a lead ridge roll with a wooden bossing stick

10-year workmanship guarantee, in writing