The pantile: one tile with a wave in it
A pantile is a single-lap roof tile with a curved, wave-like profile. Each tile has a rising curve on one side and a dip on the other, and the next tile in the row overlaps the rise of its neighbour so that rain runs down the dip and off the edge of the roof. Because the shape does the work of shedding water, a pantile roof is made of fewer, larger pieces than a roof of small flat tiles.
Both clay and concrete are used to make them. A clay tile is moulded and fired, and a concrete tile is cast from cement and sand. Both end up with the same rolling profile on the roof, so the two can look alike from the ground. Behind the shared shape, each product carries its own minimum pitch, weight and published lifespan, and those figures are not interchangeable.
Product names add to the confusion. Canterbury and Anglia are Marley products, not places and not types of roof. Marley lists a clay Lincoln pantile and a concrete Anglia tile, each with its own minimum pitch. Always check the maker's data sheet for the exact tile, and not the general name of the shape, before you compare one roof with another.
The shape explains some of what you see on a roof in repair. A broken pantile leaves a gap along the whole length of its wave, not a small hole, and a slipped one can drag its neighbours with it. A pantile covers more roof per tile than a plain tile does, which is why a repair may involve fewer tiles but each of them is bigger and heavier to handle on a slope.
Words you will meet
- PantileA wave-profile tile that laps its neighbour
- HeadlapHow far one course covers the one below
- GaugeThe spacing between battens
- PitchRoof slope, measured in degrees
- TorchingMortar pointed under the tile laps
Pantile, plain tile or interlocking tile
A plain tile is small, flat and slightly curved, and its courses overlap, so each course covers two below it. A pantile is larger and laps sideways as well as downwards. An interlocking tile has grooves along its sides that lock it to the next tile and covers a larger area per tile again. Our guide to plain tile roofs covers the first of those in detail.
The tiles ask different things of the roof under them. Marley's published minimum pitches show the spread: its Lincoln clay pantile is listed at 15 degrees, its concrete Anglia at 25 degrees, its concrete plain tile at 35 degrees and its clay Canterbury at 40 degrees. A shallow roof can take some tiles that a steep roof does not need, and a roof that is too shallow for its tile will let water back under the laps.
| Marley product | Material | Minimum pitch |
|---|---|---|
| Lincoln pantile | Clay | 15 degrees |
| Anglia | Concrete | 25 degrees |
| Plain tile | Concrete | 35 degrees |
| Canterbury | Clay | 40 degrees |
Those numbers belong to Marley's own products. Another maker's tile carries a different figure of its own, so the roof's slope is measured first and the product is chosen afterwards. Our guide to pantile pitch and headlap goes further into the numbers.
What a pantile product sheet tells you
A maker's data sheet is the document that settles how a tile is laid. Take Sandtoft's clay Old English Pantile, made by Wienerberger. Its sheet lists a minimum pitch of 30 degrees and a headlap of 75 mm. The batten gauge is fixed at 290 mm, and the weight when laid is 41.6 kg per m². Four separate figures, and each one affects the work. A tile from another maker will list different ones, so none of these can be carried across.
The pitch decides whether the tile can be used on a given roof at all. The headlap is the overlap between courses, which keeps water out where the tiles meet. The batten gauge is the spacing of the timber battens that carry the tiles, and it sets where every course sits. The weight as laid is what the roof structure has to carry, and it matters if the roof is being re-covered in a different product.
The weight point has a rule attached. The Planning Portal lists approval as needed where "You use a new covering material which increases the weight of the roof covering by 15 per cent or more." It adds that you are advised to check with a structural engineer or surveyor before starting. A tile's weight per m² is printed on the maker's data sheet, which means the comparison is made from the sheets, not from the look of the tile. Where the new covering is 15 per cent or more heavier, the approval and the structural check come first. Our guide to pitched roofing sets the whole subject in context.
Figures to find on any tile's sheet
- Minimum roof pitch
- Headlap
- Batten gauge
- Weight as laid
- Fixing method for each course
- Edge, ridge and verge parts
Dry-laid and torched pantiles
On an older roof, pantiles may be torched: a lime-based mortar pushed into the underside of the laps, from inside the roof, to seal the gaps and help hold the tiles. A roof laid without that mortar, with the tiles fixed to the battens by clips or nails, is called dry-laid. Both methods exist, and a survey from the loft shows which one you have. Where lime is visible between the battens and the tiles, the roof was torched. Where daylight can be seen at the laps, the tiles are not sealed, and that is a sign of a worn or open-laid roof rather than a failure in itself.
Fixing is where the code of practice has moved. BS 5534:2014+A2:2018 is the current standard for slating and tiling. Marley says that installing to BS 5534 isn't required by law, and also that "The 2015 amendments made it clear that mortar could no longer be relied upon as the only means of securing the roof covering." A mortar-only fixing is not a fixing that the standard relies on. For an older roof, that does not make the old work wrong, but it means that a repair or re-roof is specified to the current code, with the fixings to match the tile and the exposure of the site.
Ridge, hip and verge tiles carry their own fixing rules. BS 8612:2018 sets out how the dry-fixed versions of those parts are specified, and Marley says: "In all cases, ridge or hip tiles should be mechanically fixed to resist the calculated wind uplift force." The verge, where the roof ends at a gable wall, follows the same fixing logic as the ridge.
Working out what kind of tile you have
Standing in the garden or on the pavement opposite, you can see the profile. Counting the tiles in a row, or noting how far apart the lines of battens show through the loft rafters, gives measurements that can be matched against a product sheet. A wave that rises and dips across each tile points to a pantile, small flat tiles in rows point to plain tiles, and large flat or gently ridged tiles that run in straight lines suggest a concrete interlocking tile. The colour can mislead: concrete tiles are made in colours that resemble fired clay, and an old clay tile can have weathered to a different shade.
Looking from the ground is not enough to know the maker, the exact product or the condition of what is underneath. Reading the product name can need a closer look: some tiles carry a maker's mark on their underside, and the loft shows the back of the roof as well. A tile's size, its headlap and the batten spacing have to be measured, and the underlay and the timbers have to be checked from the loft. If you send us a photograph on WhatsApp we can tell you what the roof looks like and whether a visit is likely to settle it.
Our survey takes in every part of the roof, not only the tile that slipped. Findings come back in plain words: which tiles are loose, whether the ridge and verge are held by mortar or by fixings, what state the battens and underlay are in and what else was seen around the chimney or the valleys. After that, the quote is one written total price for the work described.
How long a pantile roof lasts
Published lifespans for tiles are estimates, not promises. For clay, Marley writes: "For clay roof tiles, the BRE determined a minimum life expectancy of 60 years". HomeBuilding's table gives clay tiles 60-80 years.
Concrete is a separate case with separate sources. HomeBuilding gives plain concrete tiles 40-50 years, and Marley writes: "Typically, roof tiles are expected to last for around 60 years", followed by "This is not a guarantee or warranty of its longevity."
HomeBuilding's concrete range sits below Marley's general figure for roof tiles. HomeBuilding's range is for plain concrete tiles, which are not pantiles, so do not read it as a pantile figure. An estimate for a material is not a forecast for a particular roof: what happens to yours turns on the fixings, the battens and underlay, the shelter it has and how it has been maintained.
- Clay tiles: HomeBuilding's 60-80 years
- Plain concrete tiles: HomeBuilding's 40-50 years
- Roof tiles in general: Marley's around 60 years, with its own caution attached
Handling and weather affect those numbers in ways no table captures. A tile that is walked on can crack, a frost can lift the surface of a poorly fired or poorly cured tile. Marley says of high-powered jet washes that they are "not recommended as it can damage the surface of the slate or tile, thus reducing its expected life considerably", which is worth knowing before anyone offers to blast a roof clean.
On cost, a typical pantile repair or re-roof depends on the roof and is priced after a survey. For figures from published sources, see our guide to what pitched roof repairs cost.